水素中에서 Ni-ZrO₂粉未成形體의 燒結收縮率에 關한 硏究
- Alternative Title
- The Densification of Nickel-Zirconia Powder Compacts in Hydrogen
- Abstract
- Ni-1.2% Zro₂紛末成形體의 燒結을 水素中에서 行하여 收縮率로부터 燒結活性化에너지를 求하였다. 그 값은 約 27,000 cal per mole이었다.
The sintering activation energy of nickel-1.2% ZrO₂powder compact has been calculated from its shrinkage in sintering. The activation energy of Ni-ZrO₂ powder compact has been evaluated to be about 27,000 cal per mole.
The sintering activation energy of nickel-1.2% ZrO₂powder compact has been calculated from its shrinkage in sintering. The activation energy of Ni-ZrO₂ powder compact has been evaluated to be about 27,000 cal per mole.
- Author(s)
- 崔性洙
- Issued Date
- 1978
- Type
- Research Laboratory
- URI
- https://oak.ulsan.ac.kr/handle/2021.oak/4660
http://ulsan.dcollection.net/jsp/common/DcLoOrgPer.jsp?sItemId=000002024344
- 공개 및 라이선스
-
- 파일 목록
-
Items in Repository are protected by copyright, with all rights reserved, unless otherwise indicated.